Temp - UP : 165 Temp - DOWN : 165 Duration : 30 min | 3 hours cooling Preparation : 1x layer, 8cm each Method : Mould frame, one load/pass Mould sheets : sanded stainless Post : Milling (sides) - 1500 RPM @ 80 facing head, 600mm/min
Temp - UP : 165 Temp - DOWN : 165 Duration : 30 min | 3 hours cooling Preparation : 1x layer, 8cm each Method : Mould frame, one load/pass Mould sheets : sanded stainless Post : Milling (sides) - 1500 RPM @ 80 facing head, 600mm/min